    Keywords: Styrene phosphonic acidcrystals ; micelle solubilization ; solubility
    Source: Springer Online Journal Archives 1860-2000
    Topics: Chemistry and Pharmacology , Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
    Notes: Abstract Some properties of styrene phosphonic acid (SPA) were studied. The crystals were triclinic, witha=0.6434 nm,b=0.5842 nm,c=2.0338 nm, α=96.17°, β=97.33°, γ=79.65° andZ=4. SPA underwent a change in crystal structure at 78.8°C, the hydrocarbon network became disordered (“liquid-like”) at 138.5°C. Crystals melted at 148.6°C giving a cubic mesophase, then changed to an isotropic liquid at 155.6°C and at 162.13°C SPA underwent decomposition. Values for pK1=2.15 and pK2=7.66 were obtained at 25°C. The water solubility of SPA at several temperatures, and its interaction with surfactant micelles were determined.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
Close ⊗
This website uses cookies and the analysis tool Matomo. More information can be found here...