Bibliothek

feed icon rss

Ihre E-Mail wurde erfolgreich gesendet. Bitte prüfen Sie Ihren Maileingang.

Leider ist ein Fehler beim E-Mail-Versand aufgetreten. Bitte versuchen Sie es erneut.

Vorgang fortführen?

Exportieren
  • 1
    Digitale Medien
    Digitale Medien
    New York, NY [u.a.] : Wiley-Blackwell
    Biotechnology and Bioengineering 28 (1986), S. 1172-1177 
    ISSN: 0006-3592
    Schlagwort(e): Chemistry ; Biochemistry and Biotechnology
    Quelle: Wiley InterScience Backfile Collection 1832-2000
    Thema: Biologie , Werkstoffwissenschaften, Fertigungsverfahren, Fertigung
    Notizen: Hydrolyses of maltose, maltotriose, and soluble starch catalyzed by glucoamylase (Asp. Niger) were carried out in the aqueous solutions of methanol, ethanol, ethylene glycol, and 1,4-dioxane at 40°C and at the optimum pH in the respective solutions. By the kinetic analysis based on the subsite model, it was shown that the intrinsic rate constant, Kint, was electrostatically affected by the dielectric constant of the hydroorganic solutions. The affinity of the third subsite, A3, which affects the apparent rate constant, K0, was correlated with the ×Gtr's of maltose and amino acid side chains.
    Zusätzliches Material: 5 Ill.
    Materialart: Digitale Medien
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
  • 2
    Digitale Medien
    Digitale Medien
    Bognor Regis [u.a.] : Wiley-Blackwell
    Journal of Polymer Science Part B: Polymer Physics 26 (1988), S. 1519-1527 
    ISSN: 0887-6266
    Schlagwort(e): Chemistry ; Polymer and Materials Science
    Quelle: Wiley InterScience Backfile Collection 1832-2000
    Thema: Chemie und Pharmazie , Physik
    Notizen: The surface coverage of porous glass (PD = 500 Å) by styrene adsorbed from its vapor (0.1-6 torr) was studied in a vacuum electrobalance. The adsorption isotherm of the monomer was analyzed by the BET method, and a full monolayer coverage was found to form at a relative pressure of 0.11, weighing 6 mg per gram of glass. Polymerization in submonolayers of adsorbed styrene was initiated by thermal decomposition of predeposited BPO and found to continue until all initiator decomposed, sample cooled, or vapor removed, hence allowing a controlled film thickness. The films were extracted in THF and analyzed by computerized GPC. Molecular weights were in the range 18000-69000. These were related to the rates of polymerization by the usual statistical correlations.
    Zusätzliches Material: 10 Ill.
    Materialart: Digitale Medien
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
Schließen ⊗
Diese Webseite nutzt Cookies und das Analyse-Tool Matomo. Weitere Informationen finden Sie hier...