ISSN:
0887-624X
Keywords:
2,7-bis(4-aminophenoxy)naphthalene
;
poly(amide-imide)s direct polycondensation
;
bis(trimellitimide)s
;
Chemistry
;
Polymer and Materials Science
Source:
Wiley InterScience Backfile Collection 1832-2000
Topics:
Chemistry and Pharmacology
Notes:
Eleven bis(phenoxy) naphthalene-containing poly(amide-imide)s IIIa-k were synthesized by the direct polycondensation of 2,7-bis (4-aminophenoxy) naphthalene (DAPON) with various aromatic bis (trimellitimide)s IIa-k in N-methyl-2-pyrrolidone (NMP) using triphenyl phosphite and pyridine as condensing agents. Poly (amide-imide)s IIIa-k having inherent viscosities of 0.70-1.12 dL/g were obtained in quantitative yields. The polymers containing p-phenylene or bis(phenoxy) benzene units exhibited crystalline x-ray diffraction patterns. Most of the polymers were readily soluble in various solvents such as NMP, N, N-dimethylacetamide, dimethyl sulfoxide, m-cresol, o-chlorophenol, and pyridine, and gave transparent, and flexible films cast from DMAc solutions. Cast films showed obvious yield points in the stress-strain curves and had strength at break up to 87 MPa, elongation to break up to 11%, and initial modulus up to 2.10 GPa. These poly(amide-imide)s had glass transition temperatures in the range of 255-321°C, and the 10% weight loss temperatures were recorded in the range of 529-586°C in nitrogen. The properties of poly(amideimide)s IIIa-k were compared with those of the corresponding isomeric poly (amide-imide)s III′ prepared from 2,7-bis(4-trimellitimidophenoxy) naphthalene and aromatic diamines. © 1994 John Wiley & Sons, Inc.
Additional Material:
3 Ill.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1002/pola.1994.080320612
Permalink