    Notes: Composite materials were made by sedimention of ceramic powders in methyl methacrylate which was then polymerized by γ-irradiation. Inclusion of 4-methacryloxyethyl trimellitic anhydride (4-META) generally was found to result in an increase in Knoop hardness number, Young's modulus, and transverse strength. Most emphasis was placed on transverse strength which was found to be increased by ca. 30% by inclusion of 4-META (5 wt %) in composites made with silanated LiAlSiO4.However an abrupt decrease in strength was found for composites with greater than ca. 83 wt % silanated LiAlSiO4. This was shown by fractography to be due to increased porosity and dewetting at the higher filler contents. Fractography also indicated that inclusion of 4-META results in a more coherent polymeric matrix. Further evidence for greater coherence was obtained by showing that 4-META confers resistance to disintegration by chloroform.
    Additional Material: 8 Ill.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
  • 2
    ISSN: 0021-9304
    Keywords: Chemistry ; Polymer and Materials Science
    Source: Wiley InterScience Backfile Collection 1832-2000
    Topics: Medicine , Technology
    Notes: The wear of a composite restorative material in the oral cavity was followed by examining impressions by scanning electron microscopy. It was demonstrated that filler particles protrude from the polymeric matrix and, eventually, are lost leaving holes in the surface. A measure of the rate of wear was obtained by following the reacession of the matrix on the faces of a large prominent particle. For a restoration that had been in place for 7 years, the average rate of wear over a further period of several months was estimated to be about 0.1 μm/day. For comparison, the gross wear of 2 mm over the entire 7-year period gives a greater average rate of wear of 0.8 μm/day.
    Additional Material: 3 Ill.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
Close ⊗
This website uses cookies and the analysis tool Matomo. More information can be found here...