    Journal of Polymer Science Part A: Polymer Chemistry 35 (1997), S. 1077-1085 
    ISSN: 0887-624X
    Keywords: s-triazine ring ; thermal stability ; polyamide ; Chemistry ; Polymer and Materials Science
    Source: Wiley InterScience Backfile Collection 1832-2000
    Topics: Chemistry and Pharmacology
    Notes: Ten new aromatic polyamides containing s-triazine rings in the main chain were synthesized by the low temperature interfacial polycondensation technique involving the reactions of each of the two s-triazine containing diacylchlorides, viz., 2,4-bis (4-chlorocarbonylphenoxy)-6-methoxy-s-triazine and 2,4-bis(3-chlorocarbonylphenoxy)-6-methoxy-s-triazine, with five aromatic diamines namely, 4,4′-bis(4-aminophenoxy)diphenyl sulfone, 4,4′-bis(3-aminophenoxy)diphenyl sulfone, 2,2-bis[4(4-aminophenoxy) phenyl] propane, 1,4 bis (4-amino-phenoxy) benzene, and 1,3-bis (4-aminophenoxy)benzene. The resulting polyamides were characterized by viscosity measurements, IR and 1H-NMR spectroscopy, solubility tests, x-ray diffraction, and thermogravimetry. The polyamides had inherent viscosities in the range of 0.16-1.06 dL/g in N,N-dimethylacetamide at 30°C. Most of the s-triazine containing polyamides dissolved readily at room temperature in polar solvents. Except for the polyamide PA-2, the polyamides did not lose weight below 350°C under a nitrogen atmosphere. © 1997 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 35: 1077-1085, 1997
    Additional Material: 4 Ill.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
Close ⊗
This website uses cookies and the analysis tool Matomo. More information can be found here...