Library

feed icon rss

Your email was sent successfully. Check your inbox.

An error occurred while sending the email. Please try again.

Proceed reservation?

Export
  • 1
    Electronic Resource
    Electronic Resource
    Springer
    Journal of materials science 25 (1990), S. 1957-1964 
    ISSN: 1573-4803
    Source: Springer Online Journal Archives 1860-2000
    Topics: Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
    Notes: Abstract Interaction between titanium and SiC particles was studied by electron microprobe, scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The distribution of the reaction products from the SiC to the titanium end is reported. Particular attention is given to the microstructure and phase analysis in areas near to the SiC. The implications of the observed microstructural and structural details are discussed.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
  • 2
    Electronic Resource
    Electronic Resource
    Weinheim [u.a.] : Wiley-Blackwell
    Materials and Corrosion/Werkstoffe und Korrosion 25 (1974), S. 663-669 
    ISSN: 0947-5117
    Keywords: Chemistry ; Polymer and Materials Science
    Source: Wiley InterScience Backfile Collection 1832-2000
    Topics: Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
    Description / Table of Contents: Über die Auslösung des Lochfraßes auf austenitischen nichtrostenden Stählen in ChioridlösungenEine Literaturübersicht hat gezeigt, daß eine Theorie, welche eine erhöhte anodische Reaktionsfähigkeit an einzelnen Punkten eines Passivfilms postuliert, mit hoher Wahrscheinlichkeit zutreffend sein dürfte. Auf Grund dieser Vermutungen wurden experimentelle Untersuchungen durchgeführt. Dabei wurde mit der Elektronenmikrosonde gezeigt, daß Chlorionen an einzelnen Punkten der Metalloberfäche bevorzugt adsorbiert werden, bevor noch Lochfraßstellen zu beobachten sind. Ferner wurde gezeigt, daß während der Induktionsperiode örtlich pH-Änderungen auftreten. Diese beiden Beobachtungen deuten darauf hin, daß schon während der Induktionsperiode Korrosion auftritt. Messungen haben jedoch gezeigt, daß die Induktionsperiode nicht gut reproduzierbar ist; besser reproduzierbar ist die pro entstehende Lochfraßstelle ubertragene Ladungsmenge vor dem Passivschichtdurchbruch. Daraus läßt sich dann die Menge der Chlorionen ermitteln, die zur Schaffung einer aktiven Stelle erforderlich ist. Messungen nach der statischen Potentialbandmethode zeigen, daß derartige Lochfraßstellen bei jedem oberhalb des Lochfraßpotentials liegenden Potentialwert entstehen können. Die entstehenden Löcher können sich jedoch auch bei jedem Potential repassivieren. Der Lochfraß beginnt danach mit der Chloridionadsorption an einzelnen Punkten, vor allem an Punkten mit örtlichen Spannungen. Die örtliche anodische Stromdichte wird dann erhöht, so daß Bedingungen (niedriger pH, hohe Chloridkonzentration) entstehen, welche die Bildung passivschichtfreier Stellen auf der Metalloberfläche begünstigen. Hierbei handelt es sich um einen autokatalytischen Prozeß. Die zur Bildung dieser Bedingungen erforderliche Zeit entspricht der beobachteten Induktionsperiode. Die Migration der aktivierenden ionen und die dadurch bedingte pH-Änderung an einem Punkt müssen einen kritischen Wert übersteigen, da sonst die den Passivfilm stabilisierenden Wirkungen überwiegen. Die hier vorgelegte Modellvorstellung stützt die Sure-Theorie und verbindet sie mit der Peptisierungstheurie.
    Notes: A literature survey has lead to the conclusion that a theory which postulates an increased anodic reactivity on a local site in the passive film is very probable. Experiments have been set up to confirm these suggestions. By means of the electron-microanalyser, it is shown that CI-ions are preferentially adsorbed at singular points at the metal surface before the stage that pits can be observed. It has also been demonstrated that pH changes occur at local areas during the induction period. These two observations indicate that corrosion already occurs during the induction period. Induction time measurements have shown that the induction time is not very reproducible. The quantity of transferred charge per initiated pit before the breakdown of the film is redly a better re- producible figure. From this, the quantity of Cl-ions necessary to create an active site is calculated. Experiments with the static potential band method reveal that pits can initiate at any potential higher than the pitting potential. Growing pits can repassivate at any potential. A model for the initiation is given. The pitting corrosion process starts with adsorption of chloride ion at singular points, mainly local stress points. The local anodic current density will be higher and in this way favourable conditions (low pH, high Cl-concentration) are created for the formation of a local site in the metal surface free of a passivating film The creation of those conditions is an autocatalytic process. The time required to form those favourable electrochemical conditions corresponds with the observed induction period. The migration of activating ions and the occurring pH change at a singular point must exceed a critical rate, otherwise passive film stabilizing effects will dominate. This model for the pitting corrosion supports the acid theory and links this theory with the peptization theory.
    Additional Material: 8 Ill.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
  • 3
    Electronic Resource
    Electronic Resource
    Weinheim [u.a.] : Wiley-Blackwell
    Materials and Corrosion/Werkstoffe und Korrosion 35 (1984), S. 37-46 
    ISSN: 0947-5117
    Keywords: Chemistry ; Polymer and Materials Science
    Source: Wiley InterScience Backfile Collection 1832-2000
    Topics: Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
    Description / Table of Contents: Korrosionsbeständigkeit von Tantallegierungen. Verhinderung der Wasserstoffsprödigkeit von Tantal durch Legieren Das Korrosionsverhalten von TaMo-, TaW-, TaNb-, TaHf-, TaZr-, TaRe-, TaNi-, TaV-, TaWMo-, TaWNb-, TaWHf- und TaWRe- Legierungen ist untersucht worden in konzentrierter Schwefelsaure bei 200 und 250°C, siedender Salzsäure der azeotropen Zusammensetzung, konzentrierter Salzsäure bei 150°C unter Druck, fluorwasserstoffhaltigen Lösungen und 0,5%iger Schwefelsäure bei Raumtemperatur (Anodisierung).In hochkorrosiven Medien wie konzentrierter Schwefelsäure bei 250°C und konzentrierter Salzsäure bei 150°C wird Tantal durch Wasserstoffaufnahme versprödet, wahrscheinlich durch die Ausscheidung von β-Hydrid, die durch mechanische Spannungen ausgelöst wird. Sowohl die Korrosionsgeschwindigkeit als auch die Wasserstoffversprödung in Schwefelsäure von 250°C werden durch Legierungselemente stark beeinflußt. Geringe Zusätze von Molybdän oder Rhenium verringern sowohl die Korrosionsgeschwindigkeit als auch die Wasserstoffversprödung, während Hafnium die gegenteilige Wirkung hat. Durch Zusatz von 1-3 At.-% Molybdän (0,5-1,5 Gew.-%) kann die Wasserstoffversprödung des Tantals in der 250°C heißen Schwefelsäure vollkommen unterbunden werden. Die erhaltenen Ergebnisse können mit Hilfe des Sauerstoffdefizits im Tantalpentoxidfilm und unter Berücksichtigung der Elektronenstruktur dieser Legierungen erschwert werden.
    Notes: The corrosion behaviour of substitutional Ta-Mo, Ta-W, Ta-Nb, Ta-Hf, Ta-Zr, Ta-Re, Ta-Ni, Ta-V, Ta-W-Mo, Ta-W-Nb, Ta-W-Hf and Ta-W-Re alloys has been investigated in various corrosive media, i.e. (1) concentrated sulfuric acid at 250°C and 200°C, (2) boiling hydrochloric acid of azeotropic composition, (3) concentrated hydrochloric acid at 150°C under pressure, (4) HF-containing solutions and (5)0.5% H2SO4 at room temperature (anodisation).In highly corrosive media such as concentrated H2SO4 at 250°C and concentrated HCl at 150°C tantalum is hydrogen embrittled, probably by stress induced precipitation of β-hydride. Both corrosion rate and hydrogen embrittlement in concentrated H2SO4 at 250°C are strongly influenced by alloying elements. Small alloying additions of either Mo or Re decrease the corrosion rate and the hydrogen embrittlement, while Hf has the opposite effect. Hydrogen embrittlement in concentrated H2SO4 at 250°C is completely eliminated by alloying Ta with 1 to 3 at % Mo (0.5 to 1.5 wt % Mo). These results can be explained in terms of the oxygen deficiency of the Ta2O5 film and the electronic structure of these alloys.
    Additional Material: 10 Ill.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...