Library

feed icon rss

Your email was sent successfully. Check your inbox.

An error occurred while sending the email. Please try again.

Proceed reservation?

Export
Filter
  • 1
    Electronic Resource
    Electronic Resource
    Springer
    Applied physics 57 (1993), S. 57-63 
    ISSN: 1432-0649
    Keywords: 43.85.+f ; 92.60.Fm
    Source: Springer Online Journal Archives 1860-2000
    Topics: Physics
    Notes: Abstract After a short review of the history of the mini-SODAR, the differences between conventinal SODAR and mini-SODARs are discussed. The background for the interpretation of the turbulent structure parameters are given. In view of existing mini-SODAR systems, some design criteria for portable systems are presented. The limitations in minimum range, vertical resolutions and velocity resolution are discussed. Results from an Arctic boundary-layer experiment, where three monostatic systems are used on a small scale, show the potential of its application. In view of other applications, future developments are presented.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
  • 2
    ISSN: 1573-4803
    Source: Springer Online Journal Archives 1860-2000
    Topics: Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
    Notes: Abstract Titanium nitride (TiN) coatings have been successfully deposited on 304 stainless steel substrates by reactive ion beam-assisted, electron beam-physical vapor deposition (RIBA, EB-PVD). The hardness values of the TiN coatings varied from 800 to 2500 VHN depending on the processing condition. The lattice parameter and hardness variation were correlated with processing parameters such as: deposition rate, bias, ion source energies, process gas, substrate temperature, and coating composition. The hardness of the TiN coatings increased with increasing ion energy. The ion energies combined with the deposition rate were the limiting factors controlling the degree of surface texturing. Surface texturing was only observed for those coatings deposited 〉8 Å/s.
    Type of Medium: Electronic Resource