Keywords:
Tl-1223
;
high-Tc superconductors
;
grain growth kinetics
;
activation energy
Source:
Springer Online Journal Archives 1860-2000
Topics:
Electrical Engineering, Measurement and Control Technology
,
Physics
Notes:
Abstract The phase formation and grain growth of (Tl,Pb,Bi)(Sr,Ba)2Ca2Cu3O9−δ ceramics were investigated in the temperature range between 860°C and 1000°C. It was found that partial melting seems to improve the texture of the samples. The phase purity, however, is limited due to an incomplete re-precipitation process due to the formation of a liquid phase, which is already present above 885°C. The resulting grain growth exponent n, however, appears to differ from the classical exponent of 1/3 for the coexistence of a liquid phase in the temperature range between 885°C and 920°C. For the first time, the activation energy for the high-Tc Tl-1223 phase has been determined showing faster grain growth kinetics than for Y-123 and Bi-2223.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1023/A:1022658602286
Permalink