The thermal properties of epoxidized natural rubber (ENR) have been found to improve upon hydrogenation in a solution phase, in the presence of a homogeneous catalyst, at 50°C. The hydrogenated ENR shows higher Tmax values in the DTG scan and, upon aging, the change in carbonyl concentration is less as compared to that of ENR, as detected by IR spectrophotometry. The hydrogenated product was characterized by IR and 1H-NMR spectroscopy. © 1993 John Wiley & Sons, Inc.