ISSN:
1436-3771
Keywords:
Key words Ceramics
;
Inlays
;
Clinical trial
;
Quantitative margin analysis
Source:
Springer Online Journal Archives 1860-2000
Topics:
Medicine
Notes:
Abstract The aim of this clinical study was to evaluate feldspathic ceramic inlays both by clinical criteria and quantitative margin analysis in continuation of an earlier, identically conducted 2-year study. Fifty feldspathic ceramic inlays were adhesively luted in Class II preparations with all margins located in enamel. The inlays were evaluated clinically according to modified USPHS criteria after 3 and 4 years. Quantitative margin analysis was performed with a scanning electron microscope (SEM). Clinically, the inlays showed no recurrent caries and no changes in colour, but superficial marginal discolouration (6%) was apparent after 4 years. Margins were perceptible clinically in 64% of the cases after 4 years. Quantitative margin analysis showed significantly more marginal gaps at the composite/ceramic interface than at the enamel/composite interface. There was neither a significant decrease in perfect margins nor a significant increase in marginal gaps and marginal imperfections at both interfaces between the third and fourth year. Clinically, the inlays performed very well up to 4 years. Clinical evaluation using an explorer only detected substance loss in the cementation gap. The SEM evaluation showed significantly higher changes in marginal qualities during the first 2-year interval of clinical service compared to the second 2-year interval following an exponential mathematical regularity. Quantitative margin analysis should be included in clinical long-term trials to detect early marginal deficiencies at the luting interfaces.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1007/s007840050028
Permalink