    Keywords: PACS: 68.55; 81.15 Z
    Source: Springer Online Journal Archives 1860-2000
    Topics: Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics , Physics
    Notes: Abstract. High-quality epitaxial CeO2 thin films were obtained on Si(001) buffered with a yttria-stabilised zirconia layer by pulsed laser deposition. Although the best structural properties were achieved at high substrate temperature, high-quality epitaxy was obtained even at room temperature. Epitaxial growth at low temperature is promoted by the high kinetic energy of particles reaching the substrate. The oxygen pressure and target–substrate distance had a strong influence on the crystallographic structure and surface morphology in low-temperature deposition. This behaviour is attributed to a change in the kinetic energy of the particles, which was evaluated from the plasma expansion velocity determined by an intensified CCD camera. If a shock wave forms, a minimum substrate temperature of 550 °C is necessary for epitaxial growth.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
  • 2
    ISSN: 1432-0630
    Keywords: PACS: 68.55; 81.15 Z
    Source: Springer Online Journal Archives 1860-2000
    Topics: Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics , Physics
    Notes: 2 (001) epitaxial thin films deposited on Si(001) with yttria-stabilized zirconia buffers have been obtained for the first time at room temperature by pulsed-laser deposition. The influence of oxygen pressure on the crystal quality of CeO2 was studied for the films deposited at 100 °C. The rocking curve full width at half maximum of the CeO2(002) peak for films deposited at room temperature and 100 °C was between 1° and 2°, for oxygen pressures below 3×10-2 mbar. The best crystal quality was obtained at around 3×10-3 mbar. Epitaxial growth at room temperature was confirmed by cross-sectional transmission electron microscopy. Scanning electron microscopy and atomic force microscopy revealed very smooth surfaces for oxygen pressure below 3×10-2 mbar, with rms roughness values around 0.3 nm over 5 μm×5 μm.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
Close ⊗
This website uses cookies and the analysis tool Matomo. More information can be found here...