    New York, NY [u.a.] : Wiley-Blackwell
    Journal of Applied Polymer Science 60 (1996), S. 2133-2140 
    ISSN: 0021-8995
    Schlagwort(e): Chemistry ; Polymer and Materials Science
    Quelle: Wiley InterScience Backfile Collection 1832-2000
    Thema: Chemie und Pharmazie , Maschinenbau , Physik
    Notizen: The thermolysis of 60/40 mixtures of polyethylene (PE) and polystyrene (PS) was investigated at temperatures below 440°C. Liquid yield from the mixture, 84.1%, was comparable to yields obtained with the individual polymers. The yields of styrene monomer, 57.1%, and α-olefins, 27.7%, increased over those obtained when the polymers were processed individually. A significant interaction was observed between the polymers in which the addition of PS enhanced the rate of thermolysis of PE. It is proposed that this enhancement was due to the abstraction of hydrogen from the PE fraction by polystyryl radicals. The result of this effect is to increase the rate of volatile production from the PE and increase the solubility of the residue in chloroform. The data also support a mechanism for dimer production other than the generally accepted 1,3 transfer. © 1996 John Wiley & Sons, Inc.
    Zusätzliches Material: 8 Ill.
    Materialart: Digitale Medien
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
  • 2
    Digitale Medien
    Digitale Medien
    New York, NY [u.a.] : Wiley-Blackwell
    Journal of Applied Polymer Science 58 (1995), S. 843-851 
    ISSN: 0021-8995
    Schlagwort(e): Chemistry ; Polymer and Materials Science
    Quelle: Wiley InterScience Backfile Collection 1832-2000
    Thema: Chemie und Pharmazie , Maschinenbau , Physik
    Notizen: Styrene was recovered from polystyrene (molecular weight of 138,000) by thermolysis in a nitrogen atmosphere at temperatures between 368 and 407°C. The results were independent of the initial weight of polystyrene, which was varied between 30 and 480 g. Up to 90% of the polystyrene was converted to liquid products. The liquid products had a styrene concentration as high as 90% and the styrene yield increased with temperature. Above 390°C, the residue left in the reactor (less than 30% of initial polystyrene charge) consisted mainly of styrene monomer, dimer, and trimer (MW of 190). The kinetics support a first-order reaction with regard to the rate of production of volatiles. The activation energy was estimated to be 166.5 kJ/mol. © 1995 John Wiley & Sons, Inc.
    Zusätzliches Material: 13 Ill.
    Materialart: Digitale Medien
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
Schließen ⊗
Diese Webseite nutzt Cookies und das Analyse-Tool Matomo. Weitere Informationen finden Sie hier...