    Keywords: alkali chloride doped ferrous oxides ; characterization ; deactivation ; oxidative activity ; oxidative coupling of methane
    Source: Springer Online Journal Archives 1860-2000
    Topics: Chemistry and Pharmacology
    Notes: Abstract In the present work, the deactivation of the NaCl/B2O3/Fe2O3 catalysts was studied for the oxidative coupling of methane. Several techniques, such as XPS, XRD, SEM, H2-TPR, and flow-reaction, were employed to examine the function of each catalyst component, and its change during the catalytic reaction. NaCl and B2O3 show a synergistic effect on the Fe2O3 surface. B2O3 modifies the oxidative activity of Fe2O3 and makes the first reduction peak of Fe2O3 shift from 490 to 750°C. The NaCl modified B2O3/Fe2O3 catalyst has high reduction rate, high activity and selectivity at about 750°C. It is demonstrated that the deactivation of the NaCl/B2O3/Fe2O3 catalysts is a complicated process, consisting of chloride loss, sodium change, B2O3 loss, silica deposition and catalyst sintering. The chloride loss enhances the surface basicity, which causes the silica deposition and sodium change, and aggravates the catalyst sintering. The silica deposition and catalyst sintering cause permanent deactivation. The B2O3 loss is not a direct reason for catalyst deactivation. NaCl crystal diluted NaCl/B2O3/Fe2O3 catalysts have a better stability. The deactivated catalyst has a more stable structure. When it is regenerated by impregnating with NaCl again, a more stable catalyst can be obtained.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
Close ⊗
This website uses cookies and the analysis tool Matomo. More information can be found here...