Library

feed icon rss

Your email was sent successfully. Check your inbox.

An error occurred while sending the email. Please try again.

Proceed reservation?

Export
  • 1
    Electronic Resource
    Electronic Resource
    Springer
    Oxidation of metals 46 (1996), S. 365-381 
    ISSN: 1573-4889
    Keywords: oxidation ; steel ; Raman ; scale ; transient oxides
    Source: Springer Online Journal Archives 1860-2000
    Topics: Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
    Notes: Abstract Using Raman scattering we have investigated the oxidation, in air, of the Fe-Cr-Ni stainless steels Fe-25Cr-20Ni, Fe-25Cr-20Ni-3Zr, and Fe-24Cr-3Zr (wt.%) as a function of temperature in the range 300 to 1000°C. The Raman technique is very sensitive to, and provides a clear identification of, the oxides Fe2O3 and Cr2O3. However, the technique is insensitive to NiO, FeO, and does not give a clear identification of spinels. The Fe−Cr−Ni alloys form chromia scales at temperatures greater than ∼800°C. At lower oxidation temperatures, transient phases are observed. With a 1-h heat treatment at 300°C, we observe the formation of an unidentified scale; we speculate that it is either amorphous or consists of disordered spinel(s). Near 400°C we begin to observe hematite (Fe2O3). The intensity of the Fe2O3 signal increases with temperature to ∼600°C and then decreases, being largely replaced by the signal from Cr2O3. The thickness of the Cr2O3 scale increases with temperature up to ∼1000°C above which spallation becomes apparent. Spinel phases also apparently persist in the scale to 1000°C.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
Close ⊗
This website uses cookies and the analysis tool Matomo. More information can be found here...