Metal surfaces of titanium, aluminum, copper, lead, and zinc were irradiated by a 25 joules pulsed laser with an energy flux ranging from 106 to 108 cal./(sq.cm.) (sec.). The resulted cavities were sectioned, polished and measured to compare with the isotherms computed from several heat conduction models. Reasonable agreement was found between the experimental cavity diameters at the interface and those calculated from the disk source model. Also, a graphical correlation between the cavity depth and its interface diameter is presented.