Bibliothek

feed icon rss

Ihre E-Mail wurde erfolgreich gesendet. Bitte prüfen Sie Ihren Maileingang.

Leider ist ein Fehler beim E-Mail-Versand aufgetreten. Bitte versuchen Sie es erneut.

Vorgang fortführen?

Exportieren
Filter
  • 2005-2009  (2)
Materialart
Erscheinungszeitraum
Jahr
  • 1
    Digitale Medien
    Digitale Medien
    Oxford, UK : Blackwell Science Ltd
    Journal of oral rehabilitation 32 (2005), S. 0 
    ISSN: 1365-2842
    Quelle: Blackwell Publishing Journal Backfiles 1879-2005
    Thema: Medizin
    Notizen: summary  The aim of this study was to evaluate in vitro dentine permeability evaluation of 2-Hydroxyethyl methacrylate (HEMA)-based desensitizing products using split-chamber model following in vivo application in the dogs for three experimental time periods of 1 week, 1 month and 3 months. Buccal enamel of upper and lower canines of nine young dogs was removed and flat dentinal surface was obtained using a water-cooled diamond bur. The dentinal surface divided into four quarters, three experimental and a control. Health-Dent and Gluma Desensitizing agent and Single bond were applied to respective quarters of one tooth, according to manufacturers’ instructions. The last quarters were left as control without any applications. For the each experimental period, 10 dentine samples from each group including control were used to measure the hydraulic conductance values. The dentine discs were placed pulp-side down in a split-chamber device in which the plastic spacers containing the rubber 0 rings have a surface area of 1 mm2 and permeability was measured by fluid filtration. The data were expressed as hydraulic conductance (Lp). Differences in dentine permeability obtained for the desensitizing agents against the control were tested for statistical significance using Kruskal–Wallis one-way anova and Bonferroni-adjusted Mann–Whitney U-tests. Differences in permeability in three time periods for each desensitizing agent were analysed using Friedman's anova and Wilcoxon signed rank tests. All desensitizing applications caused decreased Lp values compared with the control Lp value at the end of 1 week. In the 1-month samples, between the Lp values of Single bond and control, no statistical difference was found (P 〉 0·05). At the end of the 3-month period, the Gluma Desensitizing agent had the lowest the Lp value (P 〈 0·05). The result of this study is that the topical application of desensitizing agents led to decrease in dentine permeability in the dog model. The Gluma Desensitizing agent provide the more lasting tubule-occluding effect than the other material tested in this model.
    Materialart: Digitale Medien
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
  • 2
    Digitale Medien
    Digitale Medien
    Oxford, UK : Blackwell Science Ltd
    Journal of oral rehabilitation 32 (2005), S. 0 
    ISSN: 1365-2842
    Quelle: Blackwell Publishing Journal Backfiles 1879-2005
    Thema: Medizin
    Notizen: summary  This study was aimed at investigating the internal adaptation of a ceramic (Ceramco II) and two composite resin inlay materials (SureFil and 3M Filtek Z 250TM) using silicon replica technique as an indicator. Forty-five standard mesial–occlusal–distal (MOD) cavities were prepared into brass moulds by using computer numerically controlled system. Inlays were prepared according to manufacturers’ instructions with indirect methods. Replicas of the prepared cavities and inlays were produced with a polyvinyl siloxane material (Elite H-D). The spaces between inlays and cavities were filled by different coloured light-body polyvinyl siloxane material. Two parallel slices (mesio-distally) were obtained from the replicas with a sharp blade. Different coloured polyvinyl siloxane material thickness between cavity and inlay was measured at seven points (mesial, occlusal and distal). The data were evaluated with anova and Tukey's honestly significantly different (HSD) statistical tests. In the SureFil and Ceramco II groups, the sizes of the contraction gaps at mesial and distal gingival floors were greater than that of the occlusal marginal walls. In comparison of gap formation at occlusal regions, while the 3M composite group showed highest gap values (204·33 ± 75·45 μm), the Ceramco II group revealed the lowest (141·17 ± 23·66 μm) (P 〈 0·05). At the gingival floors, gap formation of Ceramco II group was the highest (227·08 ± 51·95 μm). Neither the 3M Filtek Z250 nor SureFil group showed any statistical difference between gap values of their self-occlusal and gingival floors (P 〉 0·05). In conclusion, our results showed that ceramic inlays did not confer any big advantage for internal adaptation over the composite inlays.
    Materialart: Digitale Medien
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
Schließen ⊗
Diese Webseite nutzt Cookies und das Analyse-Tool Matomo. Weitere Informationen finden Sie hier...