    Applied physics 21 (1980), S. 335-338 
    ISSN: 1432-0630
    Schlagwort(e): 75.30
    Quelle: Springer Online Journal Archives 1860-2000
    Thema: Maschinenbau , Physik
    Notizen: Abstract Ribbon-form Sendust was prepared by a roll quenching method. The size of the ribbon was 20∼110 μm thick, 2∼8 mm wide and 5∼10 m long. The normal direction of the ribbon plane was parallel to the [100] as well as the [110] axes, and no preferential directions exist within the ribbon plane. Vickers hardnessH v of the as-prepared ribbon was 563±7, decreased with increasing the annealing time and became almost constant. The minimum bending diameter of the as-prepared ribbon was 8 mm and increased gradually with increase of the annealing time. Initial permeability of the 84.80 Fe·9.50 Si·5.70 Al ribbon was about 34,000 in the frequency range from 1 to 3kHz and decreased to be 10,000 at 85 kHz. The permeability of the molded core in a resin was about 21,000 in the frequency range from 1 to 3 kHz.
    Materialart: Digitale Medien
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
Schließen ⊗
Diese Webseite nutzt Cookies und das Analyse-Tool Matomo. Weitere Informationen finden Sie hier...