References
H. N. Ko, J. Mater. Sci. LetT. 8 (1989) 1438.
Idem, ibiD. 11 (1992) 1711.
Idem, ibiD. 12 (1993) 1866.
Idem, in “Fracture mechanics of ceramics 9” (Plenum Press, New York, 1992) p. 517.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Ko, H.N., Ueno, A. Decorated pore detecting fatigue fracture origin of sintered A1203. J Mater Sci Lett 15, 1097–1099 (1996). https://doi.org/10.1007/BF00274919