Phase diagram for diamond growth in atmospheric oxyacetylene flames

  • Regular paper
  • Published:
Applied Physics A Aims and scope Submit manuscript

2

/C2H2 ratio for diamond synthesis in oxyacetylene flames can be theoretically predicted. When the substrate temperature is between 1000 K and 1250 K, the corresponding O2/C2H2 ratio range is about between 0.8 and 1.1. The suitable range of substrate temperature is widest for O2/C2H2 ratio close to unity and is narrowed rapidly when the flow ratio deviates from unity.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

Author information

Authors and Affiliations

Authors

Additional information

Received: 2 March 1997/Accepted: 17 July 1997

Rights and permissions

Reprints and permissions

About this article

Cite this article

Zhang, D., Liu, ZJ., Wan, YZ. et al. Phase diagram for diamond growth in atmospheric oxyacetylene flames . Appl Phys A 66, 49–51 (1998). https://doi.org/10.1007/s003390050636

Download citation

  • Issue Date:

  • DOI: https://doi.org/10.1007/s003390050636

Navigation