Corrosion of the alloy AlMg 2 Mn 0,8 in highly-concentrated nitric acidThe purpose of the study was to investigate the corrosion of the alloy AlMg 2 Mn 0.8 in highly-concentrated nitric acid at temperatures between 5 °C and 50°C.The corrosion rates follow the Arrhenius equation \documentclass{article}\pagestyle{empty}\begin{document}$$ \lg \ {\rm w}_{{\rm lin}} = - {\textstyle{{3170} \over {\rm T}}} + 9.1; $$\end{document} the apparent activation energy was calculated to be -60.8 kJ/mol.The ratio of the dissolved alloy components aluminum and magnesium indicates that magnesium had accumulated near the surface of the metal before the exposure to nitric acid. This finding is confirmed by surface analysis.
Notes:
Untersucht wird die Korrosion der Legierung AlMg 2 Mn 0,8 in hochkonzentrierter Salpetersäure bei Temperaturen zwischen 5 und 50°C.Die Abtragungsraten folgen der Arrhenius-Beziehung \documentclass{article}\pagestyle{empty}\begin{document}$$ \lg \ {\rm w}_{{\rm lin}} = - {\textstyle{{3170} \over {\rm T}}} + 9,1; $$\end{document} die scheinbare Aktivierungsenergie ergibt sich zu -60.8 kJ/mol.Aus dem Verhältnis der in Lösung gegangenen Legierungsanteile Aluminium und Magnesium ist abzuleiten, daß Magnesium vor der Salpetersäure-Beanspruchung in der Metalloberfläche angereichert ist. Dieser Befund wird durch oberflächenanalytische Untersuchungen bestätigt.
Additional Material:
17 Ill.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1002/maco.19860370204
Permalink