[Auszug] Argon arc melting was used to prepare the high purity alloy of composition (wt%) Ni (3.4); 119Sn (0.19); C (0.10); Fe (balance). The cast alloy was rolled to a thickness of 100 Mm, an optimum thickness for the Mossbauer measurements, and austenitised for 1 h at 1,120 C followed by a water quench. ...