Bibliothek

feed icon rss

Ihre E-Mail wurde erfolgreich gesendet. Bitte prüfen Sie Ihren Maileingang.

Leider ist ein Fehler beim E-Mail-Versand aufgetreten. Bitte versuchen Sie es erneut.

Vorgang fortführen?

Exportieren
Filter
  • 1
    Digitale Medien
    Digitale Medien
    s.l. ; Stafa-Zurich, Switzerland
    Materials science forum Vol. 480-481 (Mar. 2005), p. 453-456 
    ISSN: 1662-9752
    Quelle: Scientific.Net: Materials Science & Technology / Trans Tech Publications Archiv 1984-2008
    Thema: Maschinenbau
    Notizen: The composition and properties of powders prepared by high-energy milling of copper sulphides with silicon have been studied by methods of X-ray diffractometry and surface area measurement. The combination of several methods was utilized to develop a coherent picture of the process. The overall process of mechano-chemical transformations in copper sulphide-silicon system proceeds viacomplicated mechanism with several overlapping steps. Phase transformations in copper sulphide phases, the formation of elemetal nanocopper with X-ray determined particle size of 23 nm and creation of ternary sulphide Cu8SiS6 with anomalous surface area values are the main products of the mechanochemical reaction
    Materialart: Digitale Medien
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
  • 2
    Digitale Medien
    Digitale Medien
    Springer
    Journal of materials synthesis and processing 8 (2000), S. 287-293 
    ISSN: 1573-4870
    Schlagwort(e): MaAl2O4 ; solid-state synthesis ; conversion to spinel ; mechanochemical reaction
    Quelle: Springer Online Journal Archives 1860-2000
    Thema: Maschinenbau
    Notizen: Abstract This work presents results of the mechanochemical pretreatments of binary mixtures of hydroxides and oxides of Mg and Al powders (activated in the energy-intensive planetary ball mill for 10 h). The effect of mechanical activation on the conversion to MA spinel and on the solid-state synthesis in the temperature range 600–1200°C has been investigated. Structural changes, as a consequence of milling, were followed by X-ray diffraction analysis and the degree of conversion to spinel was determined by chemical analysis, by leaching of the products of synthesis. The aim of the intensive milling of powdery mixture has been to achieve so-called "soft" mechanical synthesis or, at least, of a partial chemical reaction, and thus, to initiate the high-temperature solid-state synthesis of MA spinel at a lower temperature than 1400°C. Pure MA spinel was prepared by synthesis of these mechanochemically activated powders at a low temperature as 1000°C. The obtained results indicate that high-energy ball milling can effectively decrease the synthesis temperature.
    Materialart: Digitale Medien
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
Schließen ⊗
Diese Webseite nutzt Cookies und das Analyse-Tool Matomo. Weitere Informationen finden Sie hier...