Conclusions To obtain the given combination of properties it is recommended that the Cu−Cr−Zr alloy be heat treated as follows: quenched from 880°, cold rolled with 90% deformation, aged at 600° for 2 h, cold worked with over 50% deformation, and annealed at 450° for 2 h.