Polymers [N(PN)4(C6H5)6N=P(C6H5)2(CH2)4P(C6H5)2]x and [N(PN)4(C6H5)6N=P-(C6H5)2C6H4C6H4P(C6H5)2]x have been formed by thermal copolymerization of trans-2,6-diazidohexaphenylcyclophosphonitrile [N3(PN)4(C6H5)6N3] with either 1,4-bis-(diphenylphosphino)butane [(C6H5)2P(CH2)4P(C6H5)2] or 4,4′-bis(diphenylphosphino)-biphenyl [(C6H5)2C6H4C6H4P(C6H5)2]. The maximum molecular weights obtained were about 10,000. A polymer endcapped with triphenyl phosphine was stable to 400°C.