The time-dependence of DP and the morphological changes on thermal degradation of linters samples subjected to different pretreatment were investigated, comparing particularly linters samples charged or not with iron. The iron content (6 mg Fe per 1 g cellulose) caused an increase of the initial rate of chain scission by one or two orders of magnitude. The resulting damages of the morphological structure, as formation of crazes or spots and separation of structural layers close to the surface, can be explained by internal stresses caused by the formation of volatile decomposition products.
Notizen:
Der zeitliche Verlauf des DP und die morphologischen Veränderungen unterschiedlich vorbehandelter Lintersproben beim thermischen Abbau wurden untersucht, wobei vor allem Fe-freie und Fe-beladene Präparate verglichen wurden. Eine Fe-Beladung (6 mg Fe/g Cellulose) erhöhte die Anfangsgeschwindigkeit der Kettenspaltung um 1 bis 2 Größenordnungen. Die auftretenden Schädigungen der morphologischen Struktur (Riß- und „Stippen“-Bildung, flächenhaftes Abheben oberflächennaher Strukturbereiche) lassen sich als Folge innerer Spannungen in Verbindung mit dem Freiwerden flüchtiger Zersetzungsprodukte deuten.
Zusätzliches Material:
9 Ill.
Materialart:
Digitale Medien
URL:
http://dx.doi.org/10.1002/actp.1981.010320502
Permalink