    Hyperfine interactions 92 (1994), S. 949-953 
    ISSN: 1572-9540
    Source: Springer Online Journal Archives 1860-2000
    Topics: Physics
    Notes: Abstract High-purity Fe powder was mechanically milled under argon at ambient temperature using an SPEX 8000 mill. The local atomic and magnetic structure was studied using57Co/Fe Mössbauer and111In/Cd perturbed angular correlations (PAC) spectroscopies. After 32 hours of milling, X-ray diffraction revealed effective grain diameters of 18 nm and energy-dispersive X-ray analysis indicated a Cr impurity concentration of ∼5%, presumably introduced by mechanical attrition of steel ball bearings used for milling. In addition to a spectral component very similar to bulk iron metal, the Mössbauer spectra exhibited hyperfine field shifts attributed to the Cr impurities. PAC spectra on Fe milled for 5 h, with no contamination, exhibited two components: (1) A slightly broadened magnetic interaction attributed to interior, defect-free sites of In/Cd probes with a mean hyperfine field slightly greater than in macroscopic grains. The defect-free site fraction grew appreciably during milling, even though In is essentially insoluble in Fe. (2) An indistinct signal due to mixed magnetic and quadrupole interactions attributed to probes at surface or other defect sites.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
Close ⊗
This website uses cookies and the analysis tool Matomo. More information can be found here...