    Electronic Resource
    Electronic Resource
    Weinheim : Wiley-Blackwell
    Angewandte Makromolekulare Chemie 163 (1988), S. 63-76 
    ISSN: 0003-3146
    Keywords: Chemistry ; Polymer and Materials Science
    Source: Wiley InterScience Backfile Collection 1832-2000
    Topics: Chemistry and Pharmacology , Physics
    Description / Table of Contents: Durch Copolymerisation von Butylacrylat (BA) mit Vinylbenzylglycidylether (VBGE) wurden neue Acrylkautschuke mit Epoxyseitengruppen hergestellt. Um die Zähigkeit eines gehärteten Epoxidharzes (Bisphenol A/Diglycidylether/p,p′-Diaminodiphenylsulfon) zu erhöhen, wurde dieses mit den erhaltenen Acrylkautschuken modifiziert. Eine Zugabe von 20 Gew.-% eines Copolymeren mit 74% BA und 26% VBGE-Einheiten führte zu einer 30proz. Zunahme der Bruchzähigkeit (KIC) des gehärteten Harzes bei einer minimalen Einbuße an Festigkeit und Steifigkeit. Die modifizierten Harze wiesen eine Zwei-Phasen-Morphologie auf, bei der Kautschukteilchen mit einer mittleren Größe von 2 μm in eine Epoxymatrix eingebettet sind. Das Copolymere ohne Epoxyseitengruppen, das aus BA und Vinylbenzylmethoxyethylether hergestellt wurde, war als Modifier unwirksam, was darauf hindeutet, daß die seitenstándigen Epoxidgruppen zu einer guten Zwischenphasenadhäsion zwischen Kautschukteilchen und Matrix, und damit zu erhöhter Zähigkeit führen. Kautschuke, die 55 oder 86% BA-Einheiten enthielten, waren ebenfalls ungenügende Modifier. Zugabe des ersteren ergab Harze mit einer homogenen Phasenstruktur, während die Zugabe des letzteren zu einer Phasentrennung zwischen Kautschuk und Epoxidharz führte.
    Notes: New acrylic rubbers with a pendant epoxy group were prepared by copolymerization of butyl acrylate (BA) with vinylbenzyl glycidyl ether (VBGE). The modification of an epoxy system (bisphenol-A diglycidyl ether/p,p′-diaminodiphenyl sulfone) with the acrylic rubbers was carried out in order to increase the toughness of the cured epoxy resin. The addition of 20 wt.-% of the copolymer containing 74% of BA and 26% of VBGE units resulted in a 30% increase in the fracture toughness (KIC) of the cured resin at minimal expenses of strength and modulus of the resin. The modified epoxy resin had two-phase morphology in which the rubber particles with average diameter of 2 μm are dispersed in the epoxy matrix. The copolymer without the pendant epoxy group, prepared from BA and vinylbenzyl methoxyethyl ether, was ineffective as a modifier, indicating that the reaction of the pendant epoxide with the epoxy matrix resulted in good interfacial adhesion between the rubber particles and the matrix, and in the increased toughness. The epoxide-containing copolymers with 55 or 86% of BA units were also insufficient modifiers. The addition of the former yielded cured resins with homogeneous structure, whereas that of the latter resulted in macroscopic phase separation between the rubber and the epoxy resin.
    Additional Material: 6 Ill.
    Type of Medium: Electronic Resource
    Library Location Call Number Volume/Issue/Year Availability
    BibTip Others were also interested in ...
Close ⊗
This website uses cookies and the analysis tool Matomo. More information can be found here...