Conclusions The use of 70–75% of silica artifacts to line steel-teeming ladles, accompanied by routine hot patchings, has permitted an increase in the lining durability by from four to five melts. With an increase in the ladle throughput from 1–2 to 6–7 melts per day, accompanied by hot patchings, the maximal lining durability was 37 melts (average 28 melts) and the refractory consumption was reduced by 2.1 kg/ton of steel. The saving obtained by the use of a silica lining was 332,200 rubles.