ISSN:
0021-8995
Keywords:
Chemistry
;
Polymer and Materials Science
Source:
Wiley InterScience Backfile Collection 1832-2000
Topics:
Chemistry and Pharmacology
,
Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
,
Physics
Notes:
Poly(α,α,α′,α′-tetrafluoro-p-xylylene) was prepared by the pyrolysis of cyclo-di-(α,α,α′,α′-tetrafluoro-p-xylylene) and by the pyrolysis of α,α′-bis(alkylsulfonyl)-α,α,α′,α′-tetrafluoro-p-xylene. The pyrolysis of α,α′-dibromo-α,α,α′,α′-tetrafluoro-p-xylylene also gave the polymer, but the method is less satisfactory. Poly(α,α,α′,α′-tetrafluoro-p-xylylene) shows remarkable thermal and oxidative stability at elevated temperatures. Useful mechanical and electrical properties are retained after aging for 3000 hr at 250° in air. After initial change due to crystallization, tensile strength remains near 10,000 psi, elongation above 5%, and dielectric constants and dissipation factors at approximately 2.4 and .001, respectively.
Additional Material:
1 Ill.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1002/app.1969.070131108